5.5.1.2  Slots   are   to   be   well-rounded   and   have   a   minimum   slot   length,  lslot,   of   75mm   and
            width, wslot, of twice the gross plate thickness. Where used in the body of doublers
            and similar locations, such welds are in general to be spaced a distance, sslot, of 2lslot
            to 3lslot but not greater than 250mm.

5.5.2.2  Slots are to be well rounded and have a minimum slot length, lslot, of 90mm and a
            minimum width, wslot, of twice the gross plate thickness. Slots cut in plating are to
            have smooth, clean and square edges and are in general to be spaced a distance, sslot,
            not greater than 140mm. Slots are not to be filled with welding.

请大家分析下这两段话 槽焊 到底是怎么定义的是: 长度75mm 宽度为 腹板板厚的两倍 最大间距不得大于250mm
                                                                  长度90mm 宽度为 腹板板厚的两倍 最大间距不得大于140mm
到底哪个是正确的 这是我在CSR 上看到的
看看大家的意见
回复

使用道具 举报

龙船学院
发表于 2010-11-9 10:36 | 显示全部楼层 来自: 中国浙江宁波
槽焊 还有间距么   槽焊不是一整条都要开掉的   英语不好看不太懂   这个会不会是关于塞焊空的要求啊  待高手来解惑
回复 支持 反对

使用道具 举报

发表于 2011-2-27 08:53 | 显示全部楼层 来自: 中国江苏南通
有大侠没?
解释一下塞焊和槽焊(slot weld)的区别。

我注意到上面有一段Slots are not to be filled with welding,什么意思槽焊不需要填满吗?